一次回火温度对烧结NdFeB永磁材料组织和性能的影响

Effect of the First Tempering on Microstructure and Properties of Sintered Nd-Fe-B Magnets

  • 摘要: 探讨了880~900℃、910~930℃、940~960℃温度区间下1h回火处理对Nd30Dy3.5Al0.2B1合金显微组织和磁性能的影响。研究表明, 温度低于910℃时, 晶界富Nd带过厚且积聚, 主相体积分数小, 矫顽力、磁能积低;温度高于930℃时, 晶粒尺寸过大, 晶界面积变小, 晶界富Nd带加厚, 矫顽力、磁能积均下降;910~930℃时晶粒尺寸趋向均匀, 晶界富Nd带呈薄层状分布, 磁性能最佳。

     

    Abstract: The effect of tempering process on the microstructure and magnetic properties of sintered Nd-Fe-B magnets were investigated.It was manifested that when the tempering temperature was below 910℃, the Nd-rich phase on grain boundary gathered and a wide band of the Nd-rich phase formed, the volume fraction of matrix phase was small and so the magnetic properties of the magnets were low.When the temperature was above 930℃, the grain size became coarse, the grain boundary area became smaller, the band of the Nd-rich phase on grain boundary became wider and the magnetic properties of the magnets were deteriorated.When the temperature is between 910℃ and 930℃, the grain size was inclined to be uniform, the content of clustered Nd-rich phase reduced, the magnetic properties of magnets were optimized.So the proper temperature for the first tempering of Nd30Dy3.5Al0.2B1 alloy shall be from 910℃ to 930℃.

     

/

返回文章
返回