KH-560改性CE/nano-SiC复合材料的韧性和耐热性

Tenacity and Heat Resistance of CE/nano-SiC Composites Modified with KH-560

  • 摘要: 采用模塑成型法制备CE/nano-SiC复合材料,通过冲击强度测试、TGA分析和DMA分析,发现偶联剂KH-560表面处理nano-SiC后,对其韧性和耐热性具有显著的协同改性作用。相对纯CE,经KH-560表面处理后的CE、1.00%nano-SiC复合材料,冲击强度提高86.26%;玻璃化转变温度提高16.71%;失重5%时,热分解温度提高17.25%;450℃时,质量保持率提高59.67%。

     

    Abstract: The CE/nano-SiC composites were made by moulding method.It was discovered that the tenacity and heat resistance of the composites were improved when the reinforcement nano-SiC was treated with coupling agent KH-560 in coordination by discussion of impact strength, TGA and DMA.Compared with CE without nano-SiC, the impact strength of the CE composite with 1.00% KH-560 treated nano-SiC increased by 86.26%, and the increase of the glass transition temperature was 16.71%. When the mass loss of composites was 5%, the heat-degradation temperature increased by 17.25%.And the quality maintaining rate increased 59.67% when its temperature was 450℃.

     

/