50Mn18Cr5钢护环开裂原因分析

Analysis on the Crack of 50Mn18Cr5 Protective Ring

  • 摘要: 采用化学成分、力学性能、断口、金相以及X射线衍射等试验方法对50Mn18Cr5钢护环开裂原因进行分析。结果表明:护环内表层产生加工硬化,形成沿晶裂纹源,材料组织不良加剧裂纹的扩展,结果导致护环在液压冷胀形的周向拉应力作用下开裂。

     

    Abstract: Chemical composition,mechanical properties,fracture and metallographic analysis were conducted to analyze the crack in the 50Mn18Cr5 protective ring.The results show that work-hardening of inner surface of the protective ring causes intercrystalline cracks,bad material structure brings about crack extention,and these lead to the fracture of the protectivering under circumferential tension stess as hydraulic bulging.

     

/