MAO Liang, MA Zhaowei, YUAN Bo, LEI Xiaowei, FU Zhanbo, DU Zhibo. Study on Laser Welding Technology of TA5 Titanium Alloy with Filler Wire[J]. Development and Application of Materials, 2022, 37(1): 66-71,76.
Citation: MAO Liang, MA Zhaowei, YUAN Bo, LEI Xiaowei, FU Zhanbo, DU Zhibo. Study on Laser Welding Technology of TA5 Titanium Alloy with Filler Wire[J]. Development and Application of Materials, 2022, 37(1): 66-71,76.

Study on Laser Welding Technology of TA5 Titanium Alloy with Filler Wire

  • Received Date: 2021-07-26
    Available Online: 2022-06-11
  • Laser welding with filler wire is adopted to realize single pass welding and double-sided forming of 4 mm thick TA5 titanium alloy with I-groove, and welding parameters on weld formation, porosity and mechanical properties are studied.Resultsshow that the welding seam is in good shape, and that the tensile strength can reach 797.5 MPa, 98.2% of that of the base metal. With the increase of laser power, the back penetration increases, the weld porosity first decreases and then increases, and the tensile strength increases. When the defocusing amount increases from negative defocusing to positive defocusing, the undercut defects disappear, the porosity first increases and then decreases, and the tensile strength increases. With the increase of welding speed, the back penetration, porosity and tensile strength decrease slightly. The results of metallographic analysis show that in weld zone, α phase has transformed to β phase completely, The rapid cooling rate after welding results in a large number of needle like α′ phase formed in weld zone during the cooling process. In heat affected zone, α phase has partially transformed to β phase was partially destroyed which is mainly made up of bulk α phase and zigzag α phase. The hardness test shows that the hardness of the weld center is the highest, that the hardness of the base metal is the lowest, meaning the hardness from the heat affected zone to the base metal zone decrease. The hardness at the top of the weld is higher than those at the center and the bottom of the weld.

     

  • loading
  • [1]
    GAO F Y,GUO Y F,QIU S W,et al.Fracture toughness of friction stir welded TA5 titanium alloy joint[J].Materials Science and Engineering:A,2020,776:138962.
    [2]
    AHN J,CHEN L,DAVIES C M,et al.Parametric optimisation and microstructural analysis on high power Yb-fibre laser welding of Ti-6Al-4V[J].Optics and Lasers in Engineering,2016,86:156-171.
    [3]
    马然,董皕喆,吴世凯,等.薄板钛合金光纤激光-钨极惰性气体保护焊电弧复合焊接工艺研究[J].中国激光,2014,41(5):85-92.
    [4]
    常辉,董月成,淡振华,等.我国海洋工程用钛合金现状和发展趋势[J].中国材料进展,2020,39(Z1):585-590.
    [5]
    吕涛,雷正龙,陈彦宾,等.焊点形状对TC4钛合金激光点焊力学性能的影响[J].中国激光,2013,40(12):51-55.
    [6]
    严铿,张培磊,蒋成禹.TA5钛合金焊接接头的低周疲劳性能[J].焊接学报,2005,26(10):84-86.
    [7]
    廖志谦,王忠平.钛合金厚板的等离子焊接[J].材料开发与应用,2005,20(4):27-28.
    [8]
    李冲健.TA5钛合金TIG焊接工艺及工艺优化模型研究[D].大连:大连理工大学,2019.
    [9]
    刘守义,王有君,耿涛.钛合金MIG焊接头组织性能[J].大连交通大学学报,2018,39(3):86-88.
    [10]
    陈彦宾.现代激光焊接技术[M].北京:科学出版社,2005.
  • 加载中

Catalog

    通讯作者: 陈斌, bchen63@163.com
    • 1. 

      沈阳化工大学材料科学与工程学院 沈阳 110142

    1. 本站搜索
    2. 百度学术搜索
    3. 万方数据库搜索
    4. CNKI搜索

    Article Metrics

    Article views (91) PDF downloads(13) Cited by()
    Proportional views
    Related

    /

    DownLoad:  Full-Size Img  PowerPoint
    Return
    Return